First of all, we have to understand what is insulation information, anti-static information, what is conductive information. Definition of insulation data: data with a specific surface resistance greater than 10 of 12 ω is considered insulation data. Insulators have very low conductivity. For this reason, the applied charge carrier remains on the surface of the data for a long time and dissipates only slowly, so that the surface of the insulator can be charged with thousands of volts without difficulty. Insulation information is not applicable to ESD use.

Definition of antistatic data: data whose specific surface resistance is between 6 OHms of 10 and 12 OHms of 10 are regarded as electrostatic dissipation data. This data can dissipate the charge carrier applied to it within a specified time. This data is for electrified data only. Data with a surface resistance of less than 10 ω is not charged.

Definition of conductive data: data with a specific surface resistance of 6 ω less than 10 are electrostatic conductive data. These materials can dissipate the charge carrier applied to them in the shortest possible time. Due to the very short discharge time, conductive materials are not suitable for all ESD applications, because the voltage peak here may cause damage, especially to electrostatic sensitive electronic components.

Secondly, PEEK data is attributed to high temperature resistant polymer special plastic, whose molding temperature is high, glass conversion temperature reaches 146 degrees; When the molding temperature is too high, there will be deformation of the profile or even it is difficult to shape, but also change the resistance value of the raw material itself, there will be conductive or anti-static together; Furthermore, the control of temperature and time of polymer materials in the annealing process is also a crucial link. The control of temperature interval and time of oven baking will affect the resistance value and volume resistance value of the profile surface.

The above is the reason why it is difficult to make anti-static information about high temperature. If you want to know more news and developments, you can click on our official website. Our company also sells POM Plastic Sheet, PEI Plastic Sheet, Abs Plastic Sheet, PEEK Plastic Sheet, PA Plastic Sheet and PC Plastic Sheet welcome customers to consult.

PEEK


HomeNewsObserve the ESD PEEK Board
Related Products List

Home

Product

Whatsapp

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send